- Place of Origin:
- Shandong, China
- Brand Name:
- bywood
- Model Number:
- 001
- Usage:
- Outdoor
- Grade:
- First-Class
- Main Material:
- Poplar
- Formaldehyde Emission Standards:
- E1
- Plywood Type:
- 1
- Core:
- Poplar Hardwood Combi
- Product name:
- LVL for packing
- Face/back:
- POPLAR
- Glue:
- MR/E0/E1/E2/WBP/Melamine
- Thickness:
- all
- Size:
- as per your requirements
- Application:
- Furniture Decoration
- Name:
- Pine LVL Scaffolding Board
- Material:
- Poplar Hardwood Finger Joint
- Color:
- Natural
- Type:
- Plywoods
- Supply Ability:
- 5000 Cubic Meter/Cubic Meters per Month
- Packaging Details
- Normal packing by pallets
- Port
- Qingdao
- Lead Time:
- 20 days
LVL for packing
Materials | poplar / hardwood / pine or as request |
glue | WBP,MR, Melamine |
Popular sizes | 38x225x3900mm/6000mm 40x235x3900mm/6000mm 42x230x3900mm/6000mm length can be up to 12000mm |
F&B | polishing,non-slip, construction workers more secure |
Edge processing | Four long edges will be chamfered to convenient and safe holding |
Profile | two sides press mark as customer"s request |
Joint way | overlap joint,end joint,scarf joint,finger joint |
Moisture content | 8%~12% |
Density | 580-620kgs/cbm |
Standard | OSHA,ANSI A10.8(US), BS24829(UK), AS1577(AUS) |
Advantage | LVL strength is three times of the same size solid wood,which is more suitable for load-bearing use |
Certificate | ISO901-2000,CE,FSC |
packing | Standard export packing |
Min order | 55cbm/40HQ |
Trade Terms | FOB,CNF,CIF,EXW |
payment | T/T or L/C at sight |
Delivery time | 15~20days after receiving the deposit or L/C |
Specifications
LVL-laminated veneer lumber:
material: poplar, pine
Density: poplar: 550kgs/cbm, pine:600 to 620kgs/cbm
LVL -laminated veneer lumber:
1,name: LVL, LVB, LVL beam, LVL batten, LVL scaffold plank, LVL plank, LVL plywood.
2, Specification:
Thickness 3mm-150mm
width: 10mm-1200mm
length: 900mm-8000mm
3,Moisture Content: less than 14%(sometimes less than 18%)
4,Glue: WBP, MR, CARB, E2,E1, E0
5,Materials: poplar, pine, combined core, birch,etc.
6,Joint: Finger joint(only used in the strict requirements for furniture usage like Door frame, not easy to bend), overlap joint(for package, furniture,etc), Scarf-joint(strong strength, for construction,etc.)
End joint(few used because of the raw plys.)
7,Density: poplar –550kgs/cbm, pine---600 to 620kgs/cbm.
8,Usage: furniture, packaging, construction,etc. It is used where the wood can be used---to take place of the wood timber! It has many advantages compared with natural wood timber----high intensity(rigidity), toughness, and good stability,easy to cut into any sizes,etc.